Indium recovery from zinc oxide flue dust by oxidative pressure leaching
LI Xuan-hai(黎铉海)1, ZHANG Yan-juan(张燕娟)1, QIN Quan-lun(覃全伦)1,
YANG Jian(阳 健)1, WEI Yan-song(韦岩松)2
(1. School of Chemistry and Chemical Engineering, Guangxi University, Nanning 530004, China;
2. Department of Chemistry and Biology, Hechi College, Yizhou 546300, China
)
Abstract: Indium was recovered from zinc oxide flue dust (ZOFD) with sulfuric acid by oxidative pressure leaching in an autoclave, and the effects of different technological conditions on indium leaching were studied. Potassium permanganate and hydrogen peroxide were used as oxidants. The atmospheric pressure leaching experiments were also carried out. The experimental results show that the leaching rate of indium can be effectively improved by oxidative pressure leaching. The optimum conditions of pressure leaching are determined as sulfuric 5.10 mol/L acid, leaching time 150 min, temperature 90 ℃, and the H2O2 dosage of 0.5 mL/g or 2.5% KMnO4. The leaching rate of indium is more than 90%, which is increased by 13% compared with that of atmospheric pressure leaching process without oxidant under the optimum conditions.
Key words: indium; zinc oxide flue dust; oxidative pressure leaching; potassium permanganate; hydrogen peroxide