Selective leaching and recovery of V as iron vanadate from industrially generated Mo-V residue
P. C. ROUT, G. K. MISHRA, D. MOHAPATRA, B. PADH, B. R. REDDY
(Technology Centre, R&D Department, Rubamin Ltd., Halol-389350, India)
Abstract: A commercial process was developed to treat a Ca-based Mo-V residue generated in Mo processing plant. Vanadium was selectively leached using acetic acid and recovered as iron vanadate by hydro process. Process conditions for selective V leaching and iron vanadate precipitation were investigated. V recovery efficiency of 90.3% was achieved with a V content of 26.5% and an Fe content of 29% in the iron vanadate cake suitable for ferrovanadium industry. The overall Mo recovery in the whole process was 98.6%. The obtained leach residue containing 14.3% Mo with negligible impurities can be used as a feed material for the Mo production process or ferromolybdenum industry. This simple and economical process generates two product streams from a single operation and has the potential to solve a long standing problem of handling such a mixed Mo-V residue.
Key words: iron vanadate; leaching; acetic acid; precipitation; ferrovanadium
Superintended by The China Association for Science and Technology (CAST)
Sponsored by The Nonferrous Metals Society of China (NFSOC)
Managed by Central South University (CSU) 湘ICP备09001153号-9