Materials Science and Engineering

Preparation of high-mechanical-property medium-entropy CrCoNi alloy by asymmetric cryorolling

Expand
  • Yu-ze WU1,2,3, Zhao-yang ZHANG1,2,3, Juan LIU1,2,3, Charlie KONG4, Yu WANG4, Puneet TANDON5, Alexander PESIN6, Hai-liang YU1,2,3
1. State Key Laboratory of High Performance Complex Manufacturing, Central South University, Changsha 410083, China;
2. College of Mechanical and Electrical Engineering, Central South University, Changsha 410083, China;
3. Light Alloys Research Institute, Central South University, Changsha 410083, China;
4. Mark Wainwright Analytical Centre, University of New South Wales, Sydney, NSW 2052, Australia;
5. PDPM Indian Institute of Information Technology, Design and Manufacturing, Jabalpur 482005, India;
6. Laboratory of Mechanics of Gradient Nanomaterials, Nosov Magnitogorsk State Technical University, Magnitogorsk 455000, Russia

Online published: 2022-05-25

Abstract

In order to obtain good strength-plasticity synergy for a medium entropy alloy (MEA) CrCoNi, cold rolling, asymmetric rolling, cryorolling and asymmetric-cryorolling with subsequent annealing at different temperatures were conducted. The results showed that the asymmetric-cryorolled alloy achieved a high strength of over 1.6 GPa. After annealing at 1073 K, it retained a high strength of ~1 GPa while the elongation reached nearly 60%. After annealing, the heterogeneous characteristics were formed in asymmetric-cryorolled samples, which were found to be more distinct than those of the samples subjected to asymmetric rolling. This resulted in the generation of high strength and ductility.

Cite this article

Yu-zeWU,Zhao-yangZHANG,JuanLIU,CharlieKONG,YuWANG,PuneetTANDON,AlexanderPESIN,Hai-liangYU, . Preparation of high-mechanical-property medium-entropy CrCoNi alloy by asymmetric cryorolling[J]. Transactions of Nonferrous Metals Society of China, 2022 , 32(5) : 1559 -1574 . DOI: 10.1016/S1003-6326(22)65893-X

Outlines

/